Power per cell
Wafer area × 1,000 W/m² standard irradiance × cell efficiency gives each cell's rated power. Capacity divided by that gives the good cells needed; line yield grosses it up to wafers.

Enter a cell or module capacity and a few process assumptions to see how many wafers, how much silicon ingot and how many quartz crucibles a year that implies. Every input is editable.
Every default is an illustrative, editable assumption, not JRST data. Results are first-pass planning estimates and must be validated against your equipment, process and supplier specifications.
Discuss wafer supply with JRSTWafer area × 1,000 W/m² standard irradiance × cell efficiency gives each cell's rated power. Capacity divided by that gives the good cells needed; line yield grosses it up to wafers.
Area × (wafer thickness + kerf) × 2.33 g/cm³. Kerf is the silicon the diamond wire turns into dust on every cut, so it counts as consumed silicon.
Brick silicon ÷ ingot-to-brick yield gives ingot grown. Enter your own polysilicon charge per crucible to estimate crucible count; the tool does not assume one.
Defaults (M10 about 330 cm², G12 about 441 cm², 24% efficiency, 130 µm wafer, 50 µm kerf, 97% line yield, 70% ingot-to-brick yield) are illustrative round numbers chosen for the worked example, not JRST production data. Real values vary by technology, wire, puller and recipe. The tool ignores melt residue, recycling of crops and squaring offcuts, breakage in handling and module-level losses. Read the background in our guides on wafer sizes, the Czochralski method and quartz crucibles, or browse wafers, crucibles and spares in our product catalogue.
It depends mainly on wafer size and cell efficiency. With the illustrative defaults on this page (M10 wafer of about 330 cm² and 24% cell efficiency) each cell is rated at roughly 7.9 W, so about 126 million good cells are needed per GW, and somewhat more wafers once line yield is allowed for. Larger wafers or higher efficiency reduce the count.
Each wafer's silicon is its area multiplied by its thickness plus the kerf lost to the wire saw, times silicon's density of about 2.33 g/cm³. Dividing the sliced-brick silicon by the ingot-to-brick yield gives the ingot that must be grown, before melt residue and recycling are considered.
No. It converts a capacity target into first-pass material quantities only. Equipment counts, pull cycles, power, consumables and economics depend on the specific process and suppliers and need a detailed engineering study.
Prepared by Mohammed Saif Zaveri, Co-Founder & Director of JRST Technology, and the JRST Industrial Advisory Team. For ingot-wafer plant setup see our ingot-wafer plant setup service; for merchant wafer or crucible enquiries use the Buyer Portal at app.jrsttechnology.com/portal.
Begin with the requirement, not a catalogue.